dc.description.abstract | Las resinas Bulk fill se pueden aplicar en incrementos de 4 a 5 mm de profundidad lo cual simplifica el proceso de restauración y reduce el tiempo clínico, por otro lado, se han realizado modificaciones en su composición lo que puede variar el desempeño clínico de las mismas. Objetivo: Evaluar la degradación y estabilidad de color de resinas Bulk fill expuestas a bebidas funcionales. Materiales y métodos: Se confeccionaron especímenes que fueron distribuidos aleatoriamente en grupos según el tipo de resina: Filtek One Bulk fill (3M ESPE), Tetric-N-Ceram Bulk fill (Ivoclar Vivadent), Filtek Z350XT (3M ESPE) las cuales fueron inmersas en las sustancias: Vita Xtra T+, On y No stress (Fuxion), Amalaki (Zrii), café (control positivo) y agua destilada (control negativo). El color fue medido al 0, 14 y 28 días después de la exposición a las sustancias, utilizando un espectofotómetro vita Easyshade Advanced 4.0 en la escala CIElab; la absorción y solubilidad fueron medidas según el ISO 4049:2009 utilizando una balanza analítica de alta precisión. Resultados: Se encontró que las bebidas On y No stress pigmentaron significativamente más que el café a los 14 y 28 días (p<0.05). En relación a la absorción, las bebidas On y No stress presentaron los menores valores de absorción en comparación con el café (p<0.05) y con respecto a solubilidad, la resina Tetric N-Ceram Bulk fill sometida a la exposición a Amalaki presentó el mayor valor de solubilidad (p<0.05). Conclusión: La bebida ON provocó cambios de color perceptibles visualmente en las resinas compuestas y la resina Filtek Z350XT mostró la menor decoloración. | es_ES |
dc.description.abstract | Bulk fill composites can be applied in increments of 4 to 5 mm of depth, which simplifies the restorative process and reduces clinical time. On the other hand, modifications have been made to their composition which may vary their clinical performance. Objective: To evaluate the degradation and color stability of Bulk fill composites exposed to functional beverages. Material and methods: Specimens were made and randomly distributed in groups according to the type of resin: Filtek One Bulk fill (3M ESPE), Tetric N-Ceram Bulk fill (Ivoclar Vivadent), Filtek Z350XT (3M ESPE) which were immersed in the substances: VitraXtra T+, On and No stress (Fuxion), Amalaki (Zrii), Coffee (positive control) and distilled water (negative control). Color was measured 0, 14 and 28 days after exposure to the substances using a vita Easyshade Advanced 4.0 spectrophotometer on the CIElab scale; sorption and solubility were measured according to ISO 4049:2009 using a high precision analytical balance. Results: On and No stress drinks pigmented significantly more than coffee at 14 and 28 days (p<0.05). In relation to sorption, On and No stress drinks presented the lowest sorption values compared to coffee (p<0.05) and with respect to solubility, Tetric N-Ceram Bulk fill resin subjected to exposure to Amalaki presented the higher solubility value (p<0.05). Conclusion: The On drink caused visually noticeabled color changes in the composite resins and the Filtek Z350XT resin showed the least discoloration. | es_ES |
dc.format | application/pdf | es_ES |
dc.language.iso | spa | es_ES |
dc.publisher | Universidad Peruana Cayetano Heredia | es_ES |
dc.rights | info:eu-repo/semantics/openAccess | es_ES |
dc.rights.uri | https://creativecommons.org/licenses/by-nc-nd/4.0/deed.es | es_ES |
dc.subject | Resinas Compuestas | es_ES |
dc.subject | Solubilidad | es_ES |
dc.subject | Color | es_ES |
dc.title | Degradación y estabilidad de color de resinas Bulk fill expuestas a bebidas funcionales | es_ES |
dc.type | info:eu-repo/semantics/masterThesis | es_ES |
thesis.degree.name | Maestro en Estomatología | es_ES |
thesis.degree.grantor | Universidad Peruana Cayetano Heredia. Escuela de Posgrado Víctor Alzamora Castro | es_ES |
thesis.degree.discipline | Estomatología | es_ES |
dc.publisher.country | PE | es_ES |
dc.subject.ocde | http://purl.org/pe-repo/ocde/ford#3.02.14 | es_ES |
renati.author.dni | 46688040 | |
renati.advisor.orcid | https://orcid.org/0000-0002-3027-178X | es_ES |
renati.advisor.orcid | https://orcid.org/0000-0002-1656-2804 | es_ES |
renati.advisor.dni | 10193841 | |
renati.advisor.dni | 41875787 | |
renati.type | https://purl.org/pe-repo/renati/type#trabajoDeInvestigacion | es_ES |
renati.level | https://purl.org/pe-repo/renati/level#maestro | es_ES |
renati.discipline | 911057 | es_ES |
renati.juror | Mas Lopez, Janett | es_ES |
renati.juror | Trevejo Pinedo, Jorge Nelson | es_ES |
renati.juror | Chavez Alayo, Pablo Armando | es_ES |