  • Quispe, Roger; Torres, Carlos; Eggert, Lara; Ccama, Gianella A.; Kurniawan, Mario; Hopfeld, Marcus; Zarate, José L.; Camargo, Magali K.; Rosenkranz, Andreas; Acosta, Julio A.; Bund, Andreas; Schaaf, Peter; Grieseler, Rolf (Wiley, 2022)
    Mn+1AXn (MAX) phases are novel structural and functional materials with a layered crystal structure. Their unique properties such as good machinability, high electrical conductivity, low friction, and corrosion resistance ...