DSpace Repository

Corrosión de arcos ortodónticos de acero y níquel- titanio sometidos a saliva artificial in vitro

Show simple item record

dc.contributor.advisor Leon Manco, Roberto Antonio es_ES
dc.contributor.author Cuevas Tenorio, Katia Emperatriz es_ES
dc.date.accessioned 2025-06-04T13:41:16Z
dc.date.available 2025-06-04T13:41:16Z
dc.date.issued 2025
dc.identifier.other 218146 es_ES
dc.identifier.uri https://hdl.handle.net/20.500.12866/17135
dc.description.abstract Introducción: Durante el tratamiento ortodóntico se emplean diferentes materiales, como los arcos, que son los dispositivos encargados de emitir fuerzas para lograr los movimientos dentarios. Estos se mantienen en la boca del paciente por intervalos prolongados desde el inicio al final del tratamiento, estando sometidos, durante estos tiempos, a una serie de agentes físicos y químicos, lo que podría contribuir a la corrosión de los componentes metálicos de los arcos, es por ello que se puede considerar normal que se presenten reacciones bioquímicas en boca, en las cuales, los aparatos se corroen. Varios de los metales que se pueden liberar están asociados a reacciones alérgicas, mutagénicas, citotóxicas y carcinogénicas. Objetivo: analizar la corrosión de las aleaciones de acero (SS) y Níquel-Titanio (NiTi) en arcos ortodónticos sometidos a saliva artificial in vitro. La muestra constará de 64 segmentos de arcos ortodónticos de acero y NiTi de las marcas comerciales American Orthodontics® (AO) y Morelli®, las cuales, serán evaluadas mediante espectrofotometría de absorción atómica después de haber sido sometidas 28 días en saliva artificial en una estufa a 37ºC. Para determinar el grado de corrosión se utilizarán 60 segmentos de alambre de 2 centímetros de longitud cada uno, de calibre 0.019x0.025”. Divididas en 2 grupos (30 segmentos de alambre) para cada marca estudiada, dentro de los cuales se tomará 15 muestras para cada tipo de aleación. Y como grupo control se tendrá un segmento perteneciente a cada subgrupo (4 segmentos). Conclusiones: Los resultados permitirán al clínico información para una mejor elección de arcos con mayor biocompatibilidad para el paciente y con menor alteración en la superficie para optimizar la biomecánica aplicada por el operador. es_ES
dc.description.abstract Introduction: During orthodontic treatment, different materials are used, such as archwires, which are the devices responsible for emitting forces to achieve dental movements. These are kept in the patient's mouth for prolonged periods from the beginning to the end of treatment, being subjected, during these times, to a series of physical and chemical agents, which could contribute to the corrosion of the metallic components of the archwires, which is why it can be considered normal that biochemical reactions occur in the mouth, in which the appliances corrode. Several of the metals that can be released are associated with allergic, mutagenic, cytotoxic and carcinogenic reactions. Objective: To analyze the corrosion of steel (SS) and Nickel-Titanium (NiTi) alloys in orthodontic archwires subjected to artificial saliva in vitro. The sample will consist of 64 segments of steel and NiTi orthodontic arches of the commercial brands American Orthodontics® (AO) and Morelli®, which will be evaluated by atomic absorption spectrophotometry after having been subjected to 28 days in artificial saliva in an oven at 37 ° C. To determine the degree of corrosion, 60 wire segments of 2 centimeters in length each, caliber 0.019x0.025 ", will be used. Divided into 2 groups (30 wire segments) for each brand studied, within which 15 samples will be taken for each type of alloy. And as a control group, there will be a segment belonging to each subgroup (4 segments). Conclusions: The results will allow the clinician to have information for a better choice of arches with greater biocompatibility for the patient and with less alteration in the surface to optimize the biomechanics applied by the operator. es_ES
dc.format application/pdf es_ES
dc.language.iso spa es_ES
dc.publisher Universidad Peruana Cayetano Heredia. es_ES
dc.rights info:eu-repo/semantics/openAccess es_ES
dc.rights.uri https://creativecommons.org/licenses/by-nc-nd/4.0/deed.es es_ES
dc.subject Corrosión es_ES
dc.subject Espectrofotometría es_ES
dc.subject Alambres para Ortodoncia es_ES
dc.title Corrosión de arcos ortodónticos de acero y níquel- titanio sometidos a saliva artificial in vitro es_ES
dc.title.alternative Corrosion of steel and nickel-titanium orthodontic arches subjected to artificial saliva in vitro es_ES
dc.type info:eu-repo/semantics/monograph es_ES
thesis.degree.name Especialista en Ortodoncia y Ortopedia Maxilar es_ES
thesis.degree.grantor Universidad Peruana Cayetano Heredia. Facultad de Estomatología Roberto Beltrán Neira es_ES
thesis.degree.discipline Ortodoncia y Ortopedia Maxilar es_ES
dc.publisher.country PE es_ES
dc.subject.ocde http://purl.org/pe-repo/ocde/ford#3.02.14 es_ES
renati.author.dni 44415652
renati.advisor.orcid https://orcid.org/0000-0001-9641-1047 es_ES
renati.advisor.dni 43649284
renati.type https://purl.org/pe-repo/renati/type#trabajoAcademico es_ES
renati.level https://purl.org/pe-repo/renati/level#tituloSegundaEspecialidad es_ES
renati.discipline 911269 es_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record

info:eu-repo/semantics/openAccess Except where otherwise noted, this item's license is described as info:eu-repo/semantics/openAccess

Search DSpace


Browse

My Account

Statistics